Castable Plus Black – Investment Friendliness Test

Posted by

                                                  R&R Ultravest vs. R&R Plasticast

 

Brass 1060oC / Flask 650oC

Investment water-powder ratio: 38:100

Flask: 3-3/8”x4” vacuum flask

Flask orientation: Keep sprue facing downward throughout the entire burnout process

Casting Machine: Vacuum Casting Machine